Dunting is a fault that can occur during the firing of ceramic articles. It is the "cracking that occurs in fired ceramic bodies as a result of a thermally induced stress" and is caused by a "ware cooled too quickly after it has been fired". Although usually occurring during cooling dunts can also be caused by excessively fast heating rates. Heating dunts can be recognised by rounded edges to the cracks as the glaze matured after they occurred, whereas cooling dunts have sharp edges.

AttributesValues
rdfs:label
  • Dunt (en)
rdfs:comment
  • Dunting is a fault that can occur during the firing of ceramic articles. It is the "cracking that occurs in fired ceramic bodies as a result of a thermally induced stress" and is caused by a "ware cooled too quickly after it has been fired". Although usually occurring during cooling dunts can also be caused by excessively fast heating rates. Heating dunts can be recognised by rounded edges to the cracks as the glaze matured after they occurred, whereas cooling dunts have sharp edges. (en)
dct:subject
Wikipage page ID
Wikipage revision ID
Link from a Wikipage to another Wikipage
sameAs
dbp:wikiPageUsesTemplate
has abstract
  • Dunting is a fault that can occur during the firing of ceramic articles. It is the "cracking that occurs in fired ceramic bodies as a result of a thermally induced stress" and is caused by a "ware cooled too quickly after it has been fired". Although usually occurring during cooling dunts can also be caused by excessively fast heating rates. Heating dunts can be recognised by rounded edges to the cracks as the glaze matured after they occurred, whereas cooling dunts have sharp edges. It has been found that bodies formulated with quartz rather than flint were more susceptible to dunting, especially on re-fire. It was postulated this may be related to the lower Young's modulus of the quartz based bodies. Dunting also occurs in wares produced from montmorillonite clay bodies due to the volume expansion of cristobalite during its inversion upon cooling. "The release of free silica, takes place in montmorillonite above 950 C, but almost double the silica is released, compared to kaolin. Therefore, clay bodies with high amounts of montmorillonite contain a high percentage of free silica after firing, which may cause the ware to crack during cooling.(Dunting)" (en)
prov:wasDerivedFrom
page length (characters) of wiki page
foaf:isPrimaryTopicOf
is Link from a Wikipage to another Wikipage of
is foaf:primaryTopic of
Faceted Search & Find service v1.17_git147 as of Sep 06 2024


Alternative Linked Data Documents: ODE     Content Formats:   [cxml] [csv]     RDF   [text] [turtle] [ld+json] [rdf+json] [rdf+xml]     ODATA   [atom+xml] [odata+json]     Microdata   [microdata+json] [html]    About   
This material is Open Knowledge   W3C Semantic Web Technology [RDF Data] Valid XHTML + RDFa
OpenLink Virtuoso version 08.03.3332 as of Dec 5 2024, on Linux (x86_64-generic-linux-glibc212), Single-Server Edition (378 GB total memory, 50 GB memory in use)
Data on this page belongs to its respective rights holders.
Virtuoso Faceted Browser Copyright © 2009-2025 OpenLink Software